MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Lubrizol LifeSciences Pellethane® 2363-80A TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pellethane 2363-80A is a thermoplastic polyurethane elastomer

Features: USP Class VI

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm0.0050 - 0.0080 in/inMD, 1.6mm thick plaques
Linear Mold Shrinkage, Transverse <= 0.0040 cm/cm<= 0.0040 in/in1.6mm thick plaques
Melt Flow 23 g/10 min
@Load 1.20 kg,
Temperature 224 °C
23 g/10 min
@Load 2.65 lb,
Temperature 435 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8181ASTM D2240
Tensile Strength, Ultimate 35.9 MPa5200 psiASTM D412
Elongation at Break 550 %550 %30% Elongation set after break; ASTM D412
50% Modulus 4.10 MPa
@Strain 50 %
4.10 MPa
@Strain 50 %
ASTM D412
100% Modulus 6.10 MPa
@Strain 100 %
885 psi
@Strain 100 %
ASTM D412
300% Modulus 12.1 MPa
@Strain 300 %
1750 psi
@Strain 300 %
ASTM D412
Tear Strength 82.3 kN/m470 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 20
@Load 1.00 kg
20
@Load 2.20 lb
H-22 (coarser); ASTM D1044
Compression Set  25 %
@Temperature 25.0 °C,
Time 79200 sec
25 %
@Temperature 77.0 °F,
Time 22.0 hour
ASTM D395
 30 %
@Temperature 70.0 °C,
Time 79200 sec
30 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
CTE, linear 170 µm/m-°C94.4 µin/in-°FASTM D696
Vicat Softening Point 85.0 °C185 °FASTM D1525
Glass Transition Temp, Tg -42.0 °C-43.6 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 210 °C379 - 410 °FMolding
Mold Temperature 15.0 - 60.0 °C59.0 - 140 °F
Drying Temperature 80.0 - 95.0 °C176 - 203 °F
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer
Lubrizol LifeSciences Pellethane® 2363-55D TPU
Lubrizol LifeSciences Pellethane® 2363-80AE TPU
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer
Lubrizol LifeSciences Pellethane® 2363-55DE TPU

PLUBR9030 / 203597

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.