MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Min-K Moldable
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Thermal Ceramics Min-K Moldable is a bulk wet form of our Min-K microporous product offering. Min-K Moldable can be extruded into shape, troweled or hand placed into areas where other insulation forms cannot be installed. Min-K Moldable requires no special curing or dry out schedule. The product can be air dried or dry time can be accelerated by applying heat to drive off water. As a microporous material, Min-K Moldable is extremely thermally efficient making it the perfect insulation for applications where space and weight are critical factors.

Min-K Moldable can be used in combination with Min-K Flexible to provide an excellent backup insulation system. Min-K Moldable allows the user to insulate around complex geometries without extensive field fabrication or complex tools.

Features:

  • Extrudable form of microporous insulation
  • Extremely thermally efficient
  • Dries to 16 pcf (256 kg/m3))density
  • Versatile placement options
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Loss On Ignition 8.0 %8.0 %
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.03234 W/m-K
    @Temperature 23.9 °C
    0.2244 BTU-in/hr-ft²-°F
    @Temperature 75.0 °F
    Dry sample thickness before test-0.431"
     0.03437 W/m-K
    @Temperature 93.3 °C
    0.2385 BTU-in/hr-ft²-°F
    @Temperature 200 °F
    Dry sample thickness before test-0.431"
     0.04699 W/m-K
    @Temperature 260 °C
    0.3261 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    Dry sample thickness before test-0.431"
     0.0715 W/m-K
    @Temperature 538 °C
    0.496 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    Dry sample thickness before test-0.431"
     0.0955 W/m-K
    @Temperature 816 °C
    0.663 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    Dry sample thickness before test-0.38"
    Maximum Service Temperature, Air 760 °C1400 °F
    Shrinkage 2.0 - 4.0 %2.0 - 4.0 %Drying shrinkage
     2.0 %
    @Temperature 649 °C,
    Time 14400 sec
    2.0 %
    @Temperature 1200 °F,
    Time 4.00 hour
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 0.41 %0.41 %
    CaO 4.71 %4.71 %
    Fe2O3 0.25 %0.25 %
    K2O <= 0.05 %<= 0.05 %
    MgO 0.90 %0.90 %
    NaO2 0.14 %0.14 %As NaO
    SiO2 75 %75 %
    TiO2 10.5 %10.5 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Thermal Ceramics Min-K 1303 Data Recorder Molded Min-K Insulation
    Thermal Ceramics Min-K 2000 Data Recorder Molded Min-K Insulation
    3M Nextel™ 610 Composite Ceramic Fiber
    Thermal Ceramics Min-K Mid Range Insulating Tape
    Thermal Ceramics Min-K Standard Insulating Tape

    CTHERM213 / 2533

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.