MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Vectran HS LCP Fiber  (discontinued **)
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes: Vectran is a high-performance thermoplastic multifilament yarn spun from liquid crystal polymer (LCP). Vectran fiber exhibits exceptional strength and rigidity. Pound for pound Vectran fiber is five times stronger than steel and ten times stronger than aluminum. These properties characterize Vectran: High strength and modulus, excellent creep resistance, high abrasion resistance, excellent flex/fold characteristics, minimal moisture absorption , excellent chemical resistance, low coefficient of thermal expansion, high dielectric strength, outstanding cut resistance, excellent property retention at high/low temperatures, outstanding vibration damping characteristics, high impact resistance.

Applications: Ropes and cables, electronics, recreations, aerospace, composites, military, industrial

Chemical Resistance: Hydrolytically stable. Resistant to organic solvents. Stable to acids (<90% conc.). Stable to bases (<30% conc.).

Information provided by Celanese Corporation. Vectran fiber is now a part of Kuraray's product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³
Moisture Absorption at Equilibrium <= 0.10 %<= 0.10 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 2840 - 3210 MPa412000 - 465000 psi10 in. gauge length, 10% strain rate, 2.5 tpi twist; ASTM D885
Elongation at Break 3.3 - 3.7 %3.3 - 3.7 %10 in. gauge length, 10% strain rate, 2.5 tpi twist; ASTM D885
Tensile Modulus 64.8 - 72.4 GPa9400 - 10500 ksi10 in. gauge length, 10% strain rate, 2.5 tpi twist; ASTM D885
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.3
@Frequency 1000 Hz
3.3
@Frequency 1000 Hz
Measured on Vectra resin
 
Thermal PropertiesMetricEnglishComments
Melting Point 330 °C626 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kuraray Vectran® HT 1500/300 LCP Fiber
Kuraray Vectran® UM 1500/300 LCP Fiber
Celanese VECTRAN™ V400P Co-Extrudable Liquid Crystal Polymer (LCP)
Celanese Vectran M LCP Fiber
Kuraray Vectran® NT 1500/300 LCP Fiber

PCELAN00 / 27949

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.