MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese VECTRAN™ V400P Co-Extrudable Liquid Crystal Polymer (LCP)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Unfilled

Material Notes: Description: PRELIMINARY DATA SHEET: Co-extrudable LCP for Barrier Applications. Vectran V400P Liquid Crystal Polymer is characterized by its excellent barrier properties independent of relative humidity, chemical resistance and contact clarity in thin film applications. This material is not suitable for medical or dental implants.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.040 %0.040 %at 50% RH; ISO 62
Moisture Vapor Transmission 0.354 cc-mm/m²-24hr-atm0.900 cc-mil/100 in²-24hr-atmat 38°C; DIN 53122-2
Oxygen Transmission 0.0315 cc-mm/m²-24hr-atm0.0800 cc-mil/100 in²-24hr-atm73°F, 100%RH; DIN 53380 part 3
 0.0354 cc-mm/m²-24hr-atm0.0900 cc-mil/100 in²-24hr-atm73°F, 100%RH; DIN 53380 part 3
Melt Flow 14 g/10 min
@Temperature 230 °C
14 g/10 min
@Temperature 446 °F
I2, nominal; Internal
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 110 °C230 °FISO 3146
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 185 - 195 °C365 - 383 °F
Middle Barrel Temperature 205 - 215 °C401 - 419 °F
Front Barrel Temperature 225 - 235 °C437 - 455 °F
Melt Temperature 225 - 235 °C437 - 455 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese VECTRAN™ V100P Co-Extrudable Liquid Crystal Polymer (LCP)
Celanese VECTRAN™ V300P Co-Extrudable Liquid Crystal Polymer (LCP)
Kuraray Vectran® HT 1500/300 LCP Fiber
Celanese VECTRAN™ V200P Co-Extrudable Liquid Crystal Polymer (LCP)
Celanese Vectran HS LCP Fiber

PHCV55 / 45896

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.