MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
34MoCr4 Alloy Steel
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel; Low Alloy Steel

Key Words: EN 10083(91)A1(96) 34MoCr4; DIN 1652(90) 34MoCr4, NMN 253-02 34MoCr4. Comparable to AISI 4137, 4135, 4130, UNS G41370, UNS G41350, UNS G41300
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1100 - 1200 MPa
@Thickness <=16.0 mm
Quenched + Tempered
Tensile Strength, Yield 800 MPa
@Thickness <=16.0 mm
Quenched + Tempered
Elongation at Break 11 %
@Thickness <=16.0 mm
Quenched + Tempered
Modulus of Elasticity 205 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel
Poissons Ratio 0.29Typical for steel
Shear Modulus 80.0 GPaTypical for steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000223 ohm-cm(AISI 4135)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.2 µm/m-°C
@Temperature 0.000 - 100 °C
(AISI 4135)
 12.4 µm/m-°C
@Temperature 0.000 - 300 °C
(AISI 4135)
 13.5 µm/m-°C
@Temperature 0.000 - 500 °C
(AISI 4135)
Specific Heat Capacity 0.477 J/g-°C(AISI 4135)
Thermal Conductivity 42.7 W/m-K(AISI 4135)
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.30 - 0.37 %
Chromium, Cr 0.90 - 1.2 %
Iron, Fe 96.4 - 97.8 %As remainder
Manganese, Mn 0.60 - 0.90 %
Molybdenum, Mo 0.15 - 0.30 %
Phosphorus, P <= 0.035 %
Silicon, Si <= 0.40 %
Sulfur, S 0.20 - 0.40 %per DIN 1652(90). S content < 0.35% per EN 10083(91)A1(96)

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 4135 Steel
JIS SCM435 Chromium Molybdenum Steel
AISI 4130 Steel, normalized at 870°C (1600°F)
AISI 4137 Steel
AISI 4130 Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round

M9Z34MoCr4 / 231095

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.