System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
MRC Polymers NAXALOY™ 780 PC+PBT Polyester Blend
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
Material Notes:
Good chemical resistance, impact and heat resistance.
Information provided by MRC Polymers Inc.
Key Words:
PC, PBT
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.20
g/cc
1.20
g/cc
solid; ASTM D792
Water Absorption
0.12 - 0.16 %
@Temperature 22.8 °C,
Time 86400 sec
0.12 - 0.16 %
@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage
0.0060
-
0.0090
cm/cm
0.0060
-
0.0090
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
58.6
MPa
8500
psi
ASTM D638
Flexural Strength
86.2
MPa
12500
psi
ASTM D790
Flexural Modulus
2.34
GPa
340
ksi
ASTM D790
Izod Impact, Notched
6.94
J/cm
13.0
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
107
°C
225
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
100
°C
212
°F
ASTM D648
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
238
-
249
°C
460
-
480
°F
Middle Barrel Temperature
243
-
254
°C
470
-
490
°F
Front Barrel Temperature
254
-
266
°C
490
-
510
°F
Nozzle Temperature
254
-
271
°C
490
-
520
°F
Melt Temperature
249
-
271
°C
480
-
520
°F
Mold Temperature
60.0
-
93.3
°C
140
-
200
°F
Drying Temperature
107
-
113
°C
225
-
235
°F
Dry Time
4
-
6
hour
4
-
6
hour
Moisture Content
<= 0.020 %
<= 0.020 %
Dew Point
<=
-17.8
°C
<=
0.000
°F
Drying Air Flow Rate
22.7
-
28.3
l/min
0.800
-
1.00
ft³/min (CFM)
per lb/hour resin processed
Injection Pressure
34.5
-
172
MPa
5000
-
25000
psi
Back Pressure
0.000
-
0.517
MPa
0.000
-
75.0
psi
Shot Size
50 - 80 %
50 - 80 %
Vent Depth
0.00127
-
0.00203
cm
0.000500
-
0.000800
in
Cushion
0.635
cm
0.250
in
Screw Speed
50
-
80
rpm
50
-
80
rpm
Descriptive Properties
Fill Rate
Moderate to Fast
Hold Pressure
40-60% of injection pressure
Packing Pressure
50-75% of injection pressure
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
RheTech Products T40P100-01A 40% Talc Reinforced Polypropylene, Black
Avient Edgetek® XT XT-100-CX01 PC+PBT
LyondellBasell Hifax TRC 779X BLK Thermoplastic Olefinic Elastomer, mineral Filled
Omni Plastics OmniCarb™ PC/PBT 400IM2 UV PC/PBT Alloy
Techmer ES Plastiblend® PC/PBT IM 1799 BK
PMRC021 / 89450
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.