MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MRC Polymers NAXALOY™ 780 PC+PBT Polyester Blend
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Good chemical resistance, impact and heat resistance.

Information provided by MRC Polymers Inc.

Key Words: PC, PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccsolid; ASTM D792
Water Absorption 0.12 - 0.16 %
@Temperature 22.8 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0060 - 0.0090 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 8500 psiASTM D638
Flexural Strength 12.5 ksiASTM D790
Flexural Modulus 340 ksiASTM D790
Izod Impact, Notched 13.0 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 225 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 212 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 460 - 480 °F
Middle Barrel Temperature 470 - 490 °F
Front Barrel Temperature 490 - 510 °F
Nozzle Temperature 490 - 520 °F
Melt Temperature 480 - 520 °F
Mold Temperature 140 - 200 °F
Drying Temperature 225 - 235 °F
Dry Time 4 - 6 hour
Moisture Content <= 0.020 %
Dew Point <= 0.000 °F
Drying Air Flow Rate 0.800 - 1.00 ft³/min (CFM)per lb/hour resin processed
Injection Pressure 5000 - 25000 psi
Back Pressure 0.000 - 75.0 psi
Shot Size 50 - 80 %
Vent Depth 0.000500 - 0.000800 in
Cushion 0.250 in
Screw Speed 50 - 80 rpm
 
Descriptive Properties
Fill RateModerate to Fast
Hold Pressure40-60% of injection pressure
Packing Pressure50-75% of injection pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RheTech Products T40P100-01A 40% Talc Reinforced Polypropylene, Black
Avient Edgetek® XT XT-100-CX01 PC+PBT
LyondellBasell Hifax TRC 779X BLK Thermoplastic Olefinic Elastomer, mineral Filled
Omni Plastics OmniCarb™ PC/PBT 400IM2 UV PC/PBT Alloy
Techmer ES Plastiblend® PC/PBT IM 1799 BK

PMRC021 / 89450

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.