MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP42HT-3AO Two part, room temperature curable epoxy system
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Key Features:
  • Convenient handling, long working life
  • Thermal conductive and electrical insulative
  • High glass transition temperature
  • Low coefficient of thermal expansion
Master Bond EP42HT-3AO is thermally conductive, electrically insulating epoxy for bonding, sealing, coating and encapsulation applications. It is relatively easy to use with a forgiving 100 to 40 mix ratio by weight. It will cure in 3-4 days at room temperature or 2-3 hours at 150-200°F. To optimize properties, the recommended curing is overnight at room temperature followed by 2-3 hours at 150-200°F. Upon mixing, EP42HT-3AO is a moderate viscosity system with very good flow properties. Among its many favorable attributes, this system has a high glass transition temperature and a low coefficient of thermal expansion. It bonds well to a wide variety of substrates including metals, composites, ceramics, glass and many plastics. Some positives include its low shrinkage upon curing and stellar dimensional stability. It is resistant to water, oils, acid, bases and many solvents. The service temperature range is from -100°F to +400°F. The color of Part A is white and the color of Part B is off-white. This blend of product properties allows this distinctive formulation to be used in specialty electronic, optical, opto-electronic, aerospace and related industries.

Product Advantages:

  • Forgiving 100:40 mix ratio by weight
  • Good flow, long working life
  • Cures at ambient and elevated temperatures
  • Superior thermal and dimensional stability
  • Very good thermal conductivity and electrical insulation
  • Combines low CTE and high Tg
  • Meets NASA low outgassing specification

Information provided by Masterbond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 500 - 1500 cP500 - 1500 cPPart B
 40000 - 80000 cP40000 - 80000 cPmixed
 750000 - 950000 cP750000 - 950000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 85 - 9585 - 95
Tensile Strength 48.3 - 55.2 MPa7000 - 8000 psi
Elongation at Break 1.0 - 3.0 %1.0 - 3.0 %
Tensile Modulus 3.79 - 4.14 GPa550 - 600 ksi
Adhesive Bond Strength 6.21 - 7.58 MPa900 - 1100 psilap shear, Al/Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 4.54.5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.0 - 16.0 µm/m-°C7.22 - 8.89 µin/in-°F
Thermal Conductivity 1.59 - 1.73 W/m-K11.0 - 12.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
Glass Transition Temp, Tg 140 - 150 °C284 - 302 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 65.6 - 93.3 °C
2.00 - 3.00 hour
@Temperature 150 - 200 °F
 4320 - 5760 min
@Temperature 23.9 °C
72.0 - 96.0 hour
@Temperature 75.0 °F
Working Life 60.0 - 90.0 min60.0 - 90.0 minAfter mixing, 100 g batch
Shelf Life 6.00 Month6.00 MonthIn original unopened containers
 
Descriptive Properties
Cure scheduleOvernight at 75°F, followed by 2-3 hours at 150-200°FOptimum
Mixing Ratio100:40Parts A to B, by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM717 / 233774

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.