MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Thermal Ceramics Superwool 607 332-E Paper
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Superwool 607 332-E Paper is a totally organic-free paper produced from Superwool 607 fibers and other special additives in a unique paper-making process. Superwool 607 332-E Paper offers excellent thermal resistance and good handling strength with no off-gassing for those mid temperature range applications. These applications would include those in appliance, non-ferrous metals, and automotive.

Features:

  • 100% organic free
  • No out-gassing
  • Low heat storage
  • Excellent strength and flexibility
  • Low thermal conductivity
  • Good fired strength
  • Easily die-cut for gasketing operations
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.176 - 0.224 g/cc0.00636 - 0.00809 lb/in³
    Loss On Ignition <= 0.50 %<= 0.50 %
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Ultimate 0.207 - 0.310 MPa30.0 - 45.0 psi
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0504 W/m-K
    @Temperature 260 °C
    0.350 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    ASTM C201
     0.0764 W/m-K
    @Temperature 538 °C
    0.530 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    ASTM C201
     0.0951 W/m-K
    @Temperature 704 °C
    0.660 BTU-in/hr-ft²-°F
    @Temperature 1300 °F
    ASTM C201
    Melting Point 982 °C1800 °F
    Maximum Service Temperature, Air 704 °C1300 °F
     
    Component Elements PropertiesMetricEnglishComments
    CaO 25 %25 %
    MgO 5.0 %5.0 %
    Other 5.0 %5.0 %
    SiO2 65 %65 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Daikin POLYFLON PA-5L PTFE Paper
    Unifrax Insulfrax® Paper
    Thermal Ceramics Kaowool 500 Paper
    DuPont™ Nomex® 410 Paper, 20 mil Nominal Thickness
    Chosun Refractories 1500 ACE PAPER Paper

    CTHERM295 / 2615

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.