MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin POLYFLON PA-5L PTFE Paper  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Papers made from POLYFLON PTFE papers are manufactured from POLYFLON PTFE fibrous powder, and do not contain any other substances. This paper is soft, elastic, and has very low gas permeability. POLYFLON PTFE papers are used as a filter for corrosive liquids, diaphragms for metal plating, and for separation of oil for oil and water mixtures.

Information provided by Daikin Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Porosity 79 %79 %Average, by volume
Thickness 519.99 microns20.472 milAverage
Pore Size <= 45.0 microns<= 1.77 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 1.40 MPa203 psiAverage
Elongation at Break 79 %79 %Average
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  1.9 - 2.1
@Frequency 1000 Hz
1.9 - 2.1
@Frequency 1000 Hz
PTFE Component; ASTM D150
 1.9 - 2.1
@Frequency 1e+6 Hz
1.9 - 2.1
@Frequency 1e+6 Hz
PTFE Component; ASTM D150
Dissipation Factor 0.00010 - 0.000220.00010 - 0.00022PTFE Component
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0PTFE Component
Oxygen Index >= 95 %>= 95 %PTFE Component

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unifrax Insulfrax® Paper
Thermal Ceramics Superwool 607 332-E Paper
Thermal Ceramics Kaowool 500 Paper
DuPont™ Nomex® 410 Paper, 20 mil Nominal Thickness
Chosun Refractories 1500 ACE PAPER Paper

PDAIK030 / 29322

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.