Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Unreinforced, Flame Retardant
Material Notes:
Notes:
Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed
Processing Method:
Injection Molding
Forms:
Pellets
Information Provided by Teknor Apex
Key Words:
Polyamide 66
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.14
g/cc
1.14
g/cc
ASTM D792
Water Absorption
1.2 %
1.2 %
24 hr; ASTM D750
Linear Mold Shrinkage
0.015
-
0.022
cm/cm
0.015
-
0.022
in/in
ASTM D955
Melt Flow
10
g/10 min
@Load 1.00 kg,
Temperature 235 °C
10
g/10 min
@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength
82.7
MPa
12000
psi
ASTM D638
Elongation at Break
50 %
50 %
ASTM D638
Elongation at Yield
5.0 %
5.0 %
ASTM D638
Flexural Strength
109
MPa
15800
psi
ASTM D790
Flexural Modulus
2.79
GPa
405
ksi
ASTM D790
Izod Impact, Notched
0.534
J/cm
@Temperature 22.8 °C
1.00
ft-lb/in
@Temperature 73.0 °F
ASTM D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+14
ohm-cm
1.00e+14
ohm-cm
ASTM D257
Dielectric Strength
18.1
kV/mm
@Thickness 3.00 mm
460
kV/in
@Thickness 0.118 in
ASTM D149
Comparative Tracking Index
600
V
600
V
UL 746
Thermal Properties
Metric
English
Comments
CTE, linear
70.2
µm/m-°C
39.0
µin/in-°F
ASTM D696
Melting Point
257
°C
495
°F
DSC
Deflection Temperature at 0.46 MPa (66 psi)
218
°C
425
°F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
87.8
°C
190
°F
Unannealed; ASTM D648
UL RTI, Electrical
115
°C
@Thickness 0.810 mm
239
°F
@Thickness 0.0319 in
UL 746
115
°C
@Thickness 1.50 mm
239
°F
@Thickness 0.0590 in
UL 746
115
°C
@Thickness 3.00 mm
239
°F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact
75.0
°C
@Thickness 0.810 mm
167
°F
@Thickness 0.0319 in
UL 746
75.0
°C
@Thickness 1.50 mm
167
°F
@Thickness 0.0590 in
UL 746
85.0
°C
@Thickness 3.00 mm
185
°F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact
95.0
°C
@Thickness 0.810 mm
203
°F
@Thickness 0.0319 in
UL 746
95.0
°C
@Thickness 1.50 mm
203
°F
@Thickness 0.0590 in
UL 746
95.0
°C
@Thickness 3.00 mm
203
°F
@Thickness 0.118 in
UL 746
Flammability, UL94
V-2
@Thickness 0.810 mm
V-2
@Thickness 0.0319 in
Oxygen Index
27 %
27 %
ASTM D2863
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
241
-
254
°C
465
-
490
°F
Middle Barrel Temperature
257
-
274
°C
495
-
525
°F
Front Barrel Temperature
263
-
282
°C
505
-
540
°F
Nozzle Temperature
263
-
279
°C
505
-
535
°F
Melt Temperature
263
-
279
°C
505
-
535
°F
Processing Temperature
Drying Temperature
79.4
°C
175
°F
Moisture Content
0.20 %
0.20 %
Descriptive Properties
Suggested Regrind, max
25
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
BASF Ultramid® A3K BK00464 PA66 (Dry)
Celanese Elvamide® 8061 PA6/66/610
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
EMS-Grivory Grilon® AZ 3/2 PA66
PTEKNO426 / 128603
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.