MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications.

Processing Method: Injection Molding

Forms: Pellets

Automotive Specifications: Ford ESB-M4D150-A; Ford ESF-M4D150-A

Information Provided by Teknor Apex

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
Water Absorption 1.2 %1.2 %24 hr; ASTM D750
Linear Mold Shrinkage 0.015 - 0.022 cm/cm0.015 - 0.022 in/inASTM D955
Melt Flow 10 g/10 min
@Load 0.325 kg,
Temperature 235 °C
10 g/10 min
@Load 0.716 lb,
Temperature 455 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 86.2 MPa12500 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Flexural Strength 110 MPa16000 psiASTM D790
Flexural Modulus 2.86 GPa415 ksiASTM D790
Izod Impact, Notched 0.587 J/cm
@Temperature 22.8 °C
1.10 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+18 ohm-cm1.00e+18 ohm-cmASTM D257
Dielectric Strength 18.1 kV/mm
@Thickness 3.00 mm
460 kV/in
@Thickness 0.118 in
ASTM D149
Comparative Tracking Index 600 V600 VUL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.2 µm/m-°C39.0 µin/in-°FASTM D696
Melting Point 257 °C495 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C195 °FUnannealed; ASTM D648
UL RTI, Electrical  115 °C
@Thickness 0.810 mm
239 °F
@Thickness 0.0319 in
UL 746
 115 °C
@Thickness 1.50 mm
239 °F
@Thickness 0.0590 in
UL 746
 115 °C
@Thickness 3.00 mm
239 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  75.0 °C
@Thickness 0.810 mm
167 °F
@Thickness 0.0319 in
UL 746
 75.0 °C
@Thickness 1.50 mm
167 °F
@Thickness 0.0590 in
UL 746
 85.0 °C
@Thickness 3.00 mm
185 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  95.0 °C
@Thickness 0.810 mm
203 °F
@Thickness 0.0319 in
UL 746
 95.0 °C
@Thickness 1.50 mm
203 °F
@Thickness 0.0590 in
UL 746
 95.0 °C
@Thickness 3.00 mm
203 °F
@Thickness 0.118 in
UL 746
Flammability, UL94 V-2V-2
Oxygen Index 27 %27 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 241 - 254 °C465 - 490 °F
Middle Barrel Temperature 257 - 274 °C495 - 525 °F
Front Barrel Temperature 263 - 282 °C505 - 540 °F
Nozzle Temperature 263 - 279 °C505 - 535 °F
Melt Temperature 263 - 279 °C505 - 535 °FProcessing Temperature
Drying Temperature 79.4 °C175 °F
Moisture Content 0.20 %0.20 %
 
Descriptive Properties
Suggested Regrind, max25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Chemlon® 109 Nylon 66, Impact Grade
Teknor Apex Chemlon® 100 W Nylon 66, Unreinforced
Celanese Zytel® 101 NC010 PA66
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer
Firestone CL200-001 Nylon 6

PTEKNO425 / 128602

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.