Forms: Pellets
Filler/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by Weight
Additive: Heat Stabilizer and Lubricant
Features: Heat Stabilized, High Temperature Strength and Lubricated
UL File Number: E157318