MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Petrothene® NA205000 Low Density Polyethylene, Extrusion Coating Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Petrothene NA205000 is an extrusion coating resin especially recommended for high-speed, light weight coating applications. The resin can be drawn to a low coating weight at line speeds in excess of 1,500 fpm with minimum neck-in and no edge weave. It is recommended for flexible pouches, locker wraps, sugar pouches, industrial and multi-wall bags and laminations.

Regulatory Status: NA205000 meets the requirements of the Food and Drug Administration regulations 21 CFR 177.1520 and 21 CFR 176.170. These regulations (respectively) allow for the use of this olefin polymer in "...articles or components of articles intended for use in contact with food;" or "as components of the uncoated or coated food-contact surface of paper and paperboard intended for use in producing, manufacturing, packaging, processing, preparing, treating, packing, transporting or holding aqueous and fatty food." Specific limitations or conditions of use may apply.

It is recommended that a melt temperature of 590°F - 620°F be used for light-weight coating applications in conjunction with electrostatic, flame or chemical priming to insure good adhesion. The maximum recommended melt temperature for NA205000 is 625°F.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Melt Flow 16 g/10 min16 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5656ASTM D2240
Tensile Strength at Break 10.3 MPa1500 psiASTM D638
Elongation at Break 640 %640 %ASTM D638
Flexural Modulus 0.212 GPa30.7 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 85.0 °C185 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 310 - 327 °C590 - 620 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem BI 818 LDPE Injection Molding Polyethylene
Chevron Phillips KN 230B LDPE Injection Molding Resin
Braskem BC818 Extrusion Coating Low Density Polyethylene
Carmel Olefins Ipethene® 111 Low Density Polyethylene
Carmel Olefins Ipethene® 100 Low Density Polyethylene

PEQU0846 / 104202

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.