MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carmel Olefins Ipethene® 111 Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: IPETHENE® 111 is a low density polyethylene extrusion grade, contains no additives. It exhibits a good balance between mechanical and optical properties.

APPLICATIONS

IPETHENE® 111 is used to produce 30 to 100 µm films for Form-Fill-Seal packaging, shrink applications, and agricultural films. It can also be used for extrusion of profiles, pipes and blow molded articles.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ISO 1183-A
Thickness 50.0 microns1.97 mil
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 250 %250 %ISO 1184
Film Elongation at Break, TD 500 %500 %ISO 1184
Elmendorf Tear Strength MD 400 g400 gISO 6283-2
Elmendorf Tear Strength TD 250 g250 gISO 6283-2
Elmendorf Tear Strength, MD 8.00 g/micron203 g/milISO 6283-2
Elmendorf Tear Strength, TD 5.00 g/micron127 g/milISO 6283-2
Dart Drop 3.60 g/micron91.4 g/milF50; ISO 7765-A
Dart Drop Test 180 g0.397 lbF50; ISO 7765-A
Film Tensile Strength at Break, MD 26.0 MPa3770 psiISO 1184
Film Tensile Strength at Break, TD 17.0 MPa2470 psiISO 1184
 
Optical PropertiesMetricEnglishComments
Haze 8.0 %8.0 %ASTM D1003
Gloss 60 %60 %45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 °C356 °F
Blow-up Ratio (BUR) 2.02.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carmel Olefins Ipethene® 322 Low Density Polyethylene
Carmel Olefins Ipethene® 320 Low Density Polyethylene
Carmel Olefins Ipethene® 214 Low Density Polyethylene
Carmel Olefins Ipethene® 213 Low Density Polyethylene
Carmel Olefins Ipethene® 210 Low Density Polyethylene

PCARM003 / 79741

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.