MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schott N-BALF5 Glass
Categories: Ceramic; Glass

Material Notes:

Information Provided by SCHOTT North America, Inc.

Key Words: 547536.261
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.61 g/cc
 
Chemical PropertiesOriginal ValueComments
Acid Class, SR 1.0
Alkali Class, AR 2.0
Stain Resistance Class, FR 0.00
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 600.1/20
Modulus of Elasticity 81.0 GPa
Poissons Ratio 0.214
Shear Modulus 33.0 GPacalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.30 µm/m-°C
@Temperature -30.0 - 70.0 °C
 8.40 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.810 J/g-°C
Thermal Conductivity 1.05 W/m-K
Transformation Temperature, Tg 558 °C
Softening Point 711 °CViscosity 107.6 dPa s
Annealing Point 559 °CViscosity 1013.0 dPa s
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.54739
@Wavelength 587.6 nm
nd
 1.54982
@Wavelength 546.1 nm
ne
Abbe Number 53.36ve
 53.63vd
Optical Dispersion 0.010207nf - nc
 0.010303nf' - nc'
Transmission, Visible 93.7 %
@Thickness 10.0 mm,
Wavelength 380 nm
 98.6 %
@Thickness 10.0 mm,
Wavelength 405 nm
 99.5 %
@Thickness 10.0 mm,
Wavelength 460 nm
 99.8 %
@Thickness 10.0 mm,
Wavelength 580 nm
 99.8 %
@Thickness 10.0 mm,
Wavelength 700 nm
IR Transmittance 61.8 %
@Thickness 10.0 mm,
Wavelength 2500 nm
 98.9 %
@Thickness 10.0 mm,
Wavelength 1530 nm
UV Transmittance 0.60 %
@Thickness 10.0 mm,
Wavelength 334 nm
 43.9 %
@Thickness 10.0 mm,
Wavelength 350 nm
 81.5 %
@Thickness 10.0 mm,
Wavelength 365 nm
 87.2 %
@Thickness 10.0 mm,
Wavelength 370 nm
 
Descriptive Properties
B1
Climatic Resistance Test CR1
HG2
K (10-6mm2/N)2.76
Phosphate Resistance PR1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott K5G20 523568.259, Optical Glass
Schott N-BAK4HT 569560.305, Optical Glass

CSGS026 / 93360

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.