Physical Properties | Metric | English | Comments |
---|
Density | 2.59 g/cc | 0.0936 lb/in³ |
|
Chemical Properties | Metric | English | Comments |
---|
Acid Class, SR | 1.0 | 1.0 |
Alkali Class, AR | 1.0 | 1.0 |
Stain Resistance Class, FR | 0.00 | 0.00 |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Knoop | 510 | 510 |
Modulus of Elasticity | 68.0 GPa | 9860 ksi |
Poissons Ratio | 0.222 | 0.222 |
Shear Modulus | 27.8 GPa | 4030 ksi |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 9.00 µm/m-°C @Temperature -30.0 - 70.0 °C | 5.00 µin/in-°F @Temperature -22.0 - 158 °F |
| 10.3 µm/m-°C @Temperature 20.0 - 300 °C | 5.72 µin/in-°F @Temperature 68.0 - 572 °F |
Specific Heat Capacity | 0.790 J/g-°C | 0.189 BTU/lb-°F |
Thermal Conductivity | 1.00 W/m-K | 6.94 BTU-in/hr-ft²-°F |
Transformation Temperature, Tg | 483 °C | 901 °F |
Softening Point | 679 °C | 1250 °F |
Annealing Point | 501 °C | 934 °F |
|
Optical Properties | Metric | English | Comments |
---|
Refractive Index | 1.497 @Wavelength 2325.4 nm | 1.497 @Wavelength 2325.4 nm |
| 1.502 @Wavelength 1970 nm | 1.502 @Wavelength 1970 nm |
| 1.507 @Wavelength 1529.6 nm | 1.507 @Wavelength 1529.6 nm |
| 1.512 @Wavelength 1060 nm | 1.512 @Wavelength 1060 nm |
| 1.513 @Wavelength 1014 nm | 1.513 @Wavelength 1014 nm |
| 1.515 @Wavelength 852.1 nm | 1.515 @Wavelength 852.1 nm |
| 1.519 @Wavelength 706.5 nm | 1.519 @Wavelength 706.5 nm |
| 1.52 @Wavelength 656.3 nm | 1.52 @Wavelength 656.3 nm |
| 1.521 @Wavelength 632.8 nm | 1.521 @Wavelength 632.8 nm |
| 1.521 @Wavelength 643.8 nm | 1.521 @Wavelength 643.8 nm |
| 1.523 @Wavelength 587.6 nm | 1.523 @Wavelength 587.6 nm |
| 1.523 @Wavelength 589.3 nm | 1.523 @Wavelength 589.3 nm |
| 1.525 @Wavelength 546.1 nm | 1.525 @Wavelength 546.1 nm |
| 1.529 @Wavelength 486.1 nm | 1.529 @Wavelength 486.1 nm |
| 1.53 @Wavelength 480 nm | 1.53 @Wavelength 480 nm |
| 1.534 @Wavelength 435.8 nm | 1.534 @Wavelength 435.8 nm |
| 1.546 @Wavelength 365 nm | 1.546 @Wavelength 365 nm |
| 1.593 @Wavelength 404.7 nm | 1.593 @Wavelength 404.7 nm |
Abbe Number | 56.47 | 56.47 |
| 56.76 | 56.76 |
Optical Dispersion | 0.009222 | 0.009222 |
| 0.009308 | 0.009308 |
Transmission, Visible | 12 % @Thickness 25.0 mm, Wavelength 680 nm | 12 % @Thickness 0.984 in, Wavelength 680 nm |
| 39 % @Thickness 25.0 mm, Wavelength 690 nm | 39 % @Thickness 0.984 in, Wavelength 690 nm |
| 44.2 % @Thickness 10.0 mm, Wavelength 680 nm | 44.2 % @Thickness 0.394 in, Wavelength 680 nm |
| 68.6 % @Thickness 10.0 mm, Wavelength 690 nm | 68.6 % @Thickness 0.394 in, Wavelength 690 nm |
| 82 % @Thickness 25.0 mm, Wavelength 420 nm | 82 % @Thickness 0.984 in, Wavelength 420 nm |
| 89 % @Thickness 25.0 mm, Wavelength 436 nm | 89 % @Thickness 0.984 in, Wavelength 436 nm |
| 92.4 % @Thickness 10.0 mm, Wavelength 420 nm | 92.4 % @Thickness 0.394 in, Wavelength 420 nm |
| 93 % @Thickness 25.0 mm, Wavelength 460 nm | 93 % @Thickness 0.984 in, Wavelength 460 nm |
| 95.4 % @Thickness 10.0 mm, Wavelength 436 nm | 95.4 % @Thickness 0.394 in, Wavelength 436 nm |
| 96.1 % @Thickness 25.0 mm, Wavelength 500 nm | 96.1 % @Thickness 0.984 in, Wavelength 500 nm |
| 97.1 % @Thickness 10.0 mm, Wavelength 460 nm | 97.1 % @Thickness 0.394 in, Wavelength 460 nm |
| 97.6 % @Thickness 25.0 mm, Wavelength 546 nm | 97.6 % @Thickness 0.984 in, Wavelength 546 nm |
| 98.2 % @Thickness 25.0 mm, Wavelength 580 nm | 98.2 % @Thickness 0.984 in, Wavelength 580 nm |
| 98.4 % @Thickness 10.0 mm, Wavelength 500 nm | 98.4 % @Thickness 0.394 in, Wavelength 500 nm |
| 98.5 % @Thickness 25.0 mm, Wavelength 620 nm | 98.5 % @Thickness 0.984 in, Wavelength 620 nm |
| 98.7 % @Thickness 25.0 mm, Wavelength 660 nm | 98.7 % @Thickness 0.984 in, Wavelength 660 nm |
| 99 % @Thickness 10.0 mm, Wavelength 546 nm | 99 % @Thickness 0.394 in, Wavelength 546 nm |
| 99.2 % @Thickness 25.0 mm, Wavelength 700 nm | 99.2 % @Thickness 0.984 in, Wavelength 700 nm |
| 99.3 % @Thickness 10.0 mm, Wavelength 580 nm | 99.3 % @Thickness 0.394 in, Wavelength 580 nm |
| 99.4 % @Thickness 10.0 mm, Wavelength 620 nm | 99.4 % @Thickness 0.394 in, Wavelength 620 nm |
| 99.5 % @Thickness 10.0 mm, Wavelength 660 nm | 99.5 % @Thickness 0.394 in, Wavelength 660 nm |
| 99.7 % @Thickness 10.0 mm, Wavelength 700 nm | 99.7 % @Thickness 0.394 in, Wavelength 700 nm |
IR Transmittance | 32 % @Thickness 25.0 mm, Wavelength 2500 nm | 32 % @Thickness 0.984 in, Wavelength 2500 nm |
| 46 % @Thickness 25.0 mm, Wavelength 2325 nm | 46 % @Thickness 0.984 in, Wavelength 2325 nm |
| 63.4 % @Thickness 10.0 mm, Wavelength 2500 nm | 63.4 % @Thickness 0.394 in, Wavelength 2500 nm |
| 73.3 % @Thickness 10.0 mm, Wavelength 2325 nm | 73.3 % @Thickness 0.394 in, Wavelength 2325 nm |
| 76 % @Thickness 25.0 mm, Wavelength 1970 nm | 76 % @Thickness 0.984 in, Wavelength 1970 nm |
| 89.6 % @Thickness 10.0 mm, Wavelength 1970 nm | 89.6 % @Thickness 0.394 in, Wavelength 1970 nm |
| 97.6 % @Thickness 25.0 mm, Wavelength 1530 nm | 97.6 % @Thickness 0.984 in, Wavelength 1530 nm |
| 98.8 % @Thickness 10.0 mm, Wavelength 1060 nm | 98.8 % @Thickness 0.394 in, Wavelength 1060 nm |
| 99 % @Thickness 10.0 mm, Wavelength 1530 nm | 99 % @Thickness 0.394 in, Wavelength 1530 nm |
| 99.5 % @Thickness 25.0 mm, Wavelength 1060 nm | 99.5 % @Thickness 0.984 in, Wavelength 1060 nm |
UV Transmittance | 2.9 % @Thickness 10.0 mm, Wavelength 370 nm | 2.9 % @Thickness 0.394 in, Wavelength 370 nm |
| 13 % @Thickness 10.0 mm, Wavelength 365 nm | 13 % @Thickness 0.394 in, Wavelength 365 nm |
| 61 % @Thickness 25.0 mm, Wavelength 400 nm | 61 % @Thickness 0.984 in, Wavelength 400 nm |
| 68 % @Thickness 25.0 mm, Wavelength 405 nm | 68 % @Thickness 0.984 in, Wavelength 405 nm |
| 82.1 % @Thickness 10.0 mm, Wavelength 400 nm | 82.1 % @Thickness 0.394 in, Wavelength 400 nm |
| 85.7 % @Thickness 10.0 mm, Wavelength 405 nm | 85.7 % @Thickness 0.394 in, Wavelength 405 nm |