MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

American Balsa Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: High buoyancy value, and good insulating value
Usual surface texture: Fine
Dimensional changes when dried lumber is subjected to variations in humidity during service: Small
Resistance to fungal decay (Heartwood in ground contact): Perishable (Under 5 years)
Resistance to penetration by preservatives: Resistant
Common Applications: Useful for heat sound and vibration insulation. Buoyancy aids

Key Words: Ochroma pyramidale; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.160 g/cc0.160 g/ccGreen
Density 0.160 g/cc0.00578 lb/in³15% Moisture Content. Density can vary by 20% or more.
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.0216 GPa3.13 ksiStatic Bending, 12% Moisture
Flexural Modulus 3.40 GPa493 ksiStatic Bending, 12% Moisture
Compressive Strength 14.9 MPa2160 psiParallel to Grain, 12% Moisture
Poissons Ratio 0.00900.0090µTL, 12% Moisture Content
 0.0180.018µRL, 12% Moisture Content
 0.2290.229µLR, 12% Moisture Content
 0.2310.231µTR, 12% Moisture Content
 0.4880.488µLT, 12% Moisture Content
 0.6650.665µRT, 12% Moisture Content
Machinability 100 %100 %Good Relative to Other Wood
Shear Strength 2.10 MPa305 psiParallel to Grain, 12% Moisture
Work to Maximum Load 0.0140 J/cm³2.03 in-lb/in³Static Bending, 12% Moisture
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0400 W/m-K0.278 BTU-in/hr-ft²-°Fat density of 0.11 g/cc; perpendicular
Shrinkage 3.0 %3.0 %Radial Shrinkage Green to Oven Dry
 7.6 %7.6 %Tangential Shrinkage Green to Oven Dry
 10.8 %10.8 %Volumetric Shrinkage Green to Oven Dry
 
Descriptive Properties
ColorWhiteUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tropical Balsa Wood
DIAB ProBalsa® PB Standard Balsa Wood
DIAB ProBalsa® LD7 Light Weight Balsa Wood
American Red Oak Wood
Carbon-Core Carbon Balsa Wood

PTSA670 / 71273

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.