MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
J6 Polymers JFOAM™ S-1200 Engineered Specialty Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: JFoam™ S-1200-R is the resin component of a two part polyurethane system, which when combined with the T component, Isocyanate, will produce a water-blown rigid polyurethane spray foam system. S-1200 can be sprayed in place or in layers for use in prototyping and tooling applications

Information provided by J6 Polymers LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccR Component, Polyol Blend
 1.24 g/ccT Component, Polymeric MDI
 11.7 lb/ft³Free Rise Cup Density, P4325
 11.76 lb/ft³Core; ASTM D1622
Water Absorption 1.27 %by volume; ASTM D2842
Viscosity 200 cPT Component, Polymeric MDI
 1100 cPR Component, Polyol Blend
Storage Temperature 65.0 - 85.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 201.2 psiParallel; ASTM D1623
Tensile Modulus 7903 psiASTM D1623
Compressive Strength 263.1 psiPerpendicular, 10% deflection; ASTM D1621
Compressive Modulus 6114 psiParallel; ASTM D1621
Shear Modulus 1.39 ksiASTM C273
Shear Strength 156 psiParallel; ASTM C273
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Closed Cell Content92.6%
Dimensional Stability+0.49% Change7 days at 70°C, 100% RH, ASTM D2126
 -0.07% Change1 day at -29°C, ASTM D2126
 -0.07% Change7 days at -29°C, ASTM D2126
 -0.07% Change14 days at -29°C, ASTM D2126
 -0.17% Change28 days at -29°C, ASTM D2126
 -0.24% Change1 day at 70°C, 100% RH, ASTM D2126
 -0.4% Change14 days at 70°C, 100% RH, ASTM D2126
 -0.46% Change1 day at 70°C, ASTM D2126
 -0.62% Change28 days at 70°C, 100% RH, ASTM D2126
 -0.77% Change7 days at 70°C, ASTM D2126
 -1.1% Change14 days at 70°C, ASTM D2126
 -1.31% Change28 days at 70°C, ASTM D2126
Friability0.0145ASTM C421
Hand Mix Reactivity6 secCream Time
Mixing Ratio0.463T Component, Polymeric MDI
 0.537R Component, Polyol Blend

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Synfoam® LG-20 Syntactic Foam
Solvay Chemicals IXOL® M 125
Sawbones Solid Rigid Polyurethane Foam 40 pcf Density
Saint-Gobain Korel® K40-35 Medium Deflection Micro-cellular Polyurethane Foam
General Plastics LAST-A-FOAM® FR-7108 Polyurethane Foam

PJSIX039 / 190966

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.