MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay Chemicals IXOL® M 125
Categories: Fluid

Material Notes: The polyol IXOL® M125 is a halogenated aliphatic polyether diol. Due to its low functionality, IXOL® M125 is particularly suited for one component polyurethane (PUR) foams or for polyisocyanurate (PIR: PUR foams modified with isocyanurate structures) foams to meet high standards in fire safety. Being a reactive compound, IXOL® M125 polyol guarantees a permanent flame retardant effect since the halogens are chemically bound to the final polymer..

CAS-No.: 86675-46-9

Uses: Flame retardants and fire preventing agents

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³
Viscosity 2900 cP2900 cP
Molecular Weight 468 g/mol468 g/mol
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.30<= 0.30[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Melting Point -44.0 - -37.0 °C-47.2 - -34.6 °F
Decomposition Temperature >= 150 °C>= 302 °F
Flash Point 198 °C388 °Fopen cup
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %
 
Component Elements PropertiesMetricEnglishComments
Bromine, Br 32.0 %32.0 %
Chlorine, Cl 7.0 %7.0 %
 
Descriptive Properties
Appearanceviscous liquid, hygroscopic
Colordark brown
Composition>99%Halogenated polyetherpolyol M 125
Hydroxyl number239[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Isoflon PUR Polyurethane
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
General Plastics LAST-A-FOAM® FR-7108 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3840 FST Polyurethane Foam
General Plastics LAST-A-FOAM® FP-5018 Polyurethane Foam

WSOLV064 / 147713

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.