MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Carmel Olefins CARMELTECH™ QB 79 P Polypropylene Random Copolymer for Pressure Pipe  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: CARMELTECH™ QB 79 P is a high molecular weight, low melt flow rate polypropylene random copolymer, especially designed for extrusion of pressure pipes and injection molding of fittings. This grade offers a combination of ease of processing and excellent mechanical properties. It has been formulated for long term heat stabilization and good resistance to extraction by hot water and detergents.

APPLICATIONS

CARMELTECH™ QB 79 P is suitable for in-house hot and cold water pipes and fittings, floor and wall heating systems, radiator connections, and industrial applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow  0.28 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.28 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 0.50 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.50 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
 1.2 g/10 min
@Load 5.00 kg,
Temperature 230 °C
1.2 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.0 MPa3340 psiASTM D638
Elongation at Yield 13 %13 %ASTM D638
Flexural Modulus 0.950 GPa138 ksiASTM D790
Izod Impact, Notched  0.850 J/cm
@Temperature >=0.000 °C
1.59 ft-lb/in
@Temperature >=32.0 °F
ASTM D256
 3.00 J/cm
@Temperature >=23.0 °C
5.62 ft-lb/in
@Temperature >=73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FASTM D648
Vicat Softening Point 133 °C
@Load 1.02 kg
271 °F
@Load 2.25 lb
ASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyMirae Moplen EP332C Pipe Extrusion Grade Polypropylene
Borealis RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems
Phillips Sumika Marlex® JM97A Polypropylene Random Copolymer, UV Stabilized
BP Amoco 8410 Polypropylene Random Copolymer
Braskem RP350 Polypropylene Random Copolymer

PCARM034 / 79772

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.