MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips Sumika Marlex® JM97A Polypropylene Random Copolymer, UV Stabilized  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Characteristics:
  • Meets FDA Regulation 21 CFR 177.1520 and is suitable for food packaging applications at temperatures not exceeding 100°C

Applications:

  • Food containers
  • Large storage boxes
  • Deli containers
  • ISBM bottles

Information provided by Chevron Phillips.

Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued prior to the shutdown announcement.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.898 g/cc
@Thickness 3.17 mm
0.0324 lb/in³
@Thickness 0.125 in
injection molded specimen; ASTM D1505
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 86
@Thickness 3.17 mm
86
@Thickness 0.125 in
injection molded sample; ASTM D785
Tensile Strength, Yield 25.5 MPa3700 psi2 in/min, 1/8" thick injection molded, type 1 specimen; ASTM D638
Flexural Modulus 0.965 GPa140 ksi1/8" thick injection molded specimen, 0.5 in/min, Tangent method; ASTM D790
Izod Impact, Notched 0.590 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
1.11 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
injection molded specimen; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 63.0 °C
@Thickness 3.17 mm
145 °F
@Thickness 0.125 in
injection molded specimen; ASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem RP350 Polypropylene Random Copolymer
Phillips 66 COPYLENE® CR120LN Polypropylene, Random Copolymer, Nucleated
Braskem DS6D82 Polypropylene Random Copolymer
Phillips 66 COPYLENE® CR020CL Polypropylene Impact Copolymer
Dow DS6D82 Polypropylene Random Copolymer Resin

PCHEVD098 / 20675

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.