MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ITW Devcon® DEVWELD 531 Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Devweld 531 is a two-part 1:1 ratio methacrylate adhesive designed for structural bonding of thermoplastic, metal and composite assemblies. Devweld 531 is particularly well suited for bonding thermoplastic materials and combines high strength and stiffness with the ability to adhere difficult-to-bond materials.

FEATURES: • Excellent shear, peel and impact strength • Non-sagging • Will fill gaps of up to 4mm • Excellent load bearing qualities • Resistant to weathering and humidity • Specifically designed for difficult-to-bond substrates • Room temperature cure • No surface preparation • 100% reactive.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.971 g/cc0.0351 lb/in³Part B, Uncured
 1.00 g/cc0.0361 lb/in³Mixed, uncured
 1.03 g/cc0.0372 lb/in³Part A, Uncured
Viscosity 40000 - 60000 cP40000 - 60000 cPPart A
 40000 - 60000 cP40000 - 60000 cPPart B
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 27.0 - 31.0 MPa3920 - 4500 psi
Elongation at Break 5.0 - 15 %5.0 - 15 %
Adhesive Bond Strength 20.0 - 24.0 MPa2900 - 3480 psiLap Shear; Cured. GBS
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 49.4 °C121 °F
Minimum Service Temperature, Air -48.3 °C-55.0 °F
Flash Point -12.8 °C9.00 °FUncured
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourFull
Pot Life 15.0 - 18.0 min15.0 - 18.0 min
 
Descriptive Properties
Chemical/Solvent ResistanceAcids and bases: excellent
 Hydrocarbons: excellent
 salt solution: excellent
Coloroff whitePart A
 yellowPart B
Fixture Time (mins)30 to 35uncured
Gap Filling (in)0.0394 to 0.157
Mix Ratio by volume1:1Part A: Part B
Mix Ratio by weight1:1Part A: Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWD9233 / 239742

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.