MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont™ Tedlar® TWH15BL3 Low Gloss White Polyvinyl Fluoride Film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer

Material Notes: Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety of chemicals, solvents, and staining agents.

Key Words: PVF
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.46 g/cc1.46 g/ccASTM D1505
Moisture Absorption at Equilibrium <= 0.50 %<= 0.50 %ASTM D570
Moisture Vapor Transmission 0.930 cc-mm/m²-24hr-atm2.36 cc-mil/100 in²-24hr-atmASTM E96
Thickness 38.1 microns1.50 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD >= 90 %>= 90 %ASTM D882
Secant Modulus, MD 2.10 GPa305 ksiASTM D822
Impact 42.742.7kJ/m; Spencer; ASTM D3420
Coefficient of Friction 0.180.18Film:Metal; ASTM D1894
Tear Strength 102 kN/m582 pliGraves (initial), TD; ASTM D1004
 129 kN/m736 pliGraves (initial), MD; ASTM D1004
Elmendorf Tear Strength, MD 0.909 g/micron23.1 g/milASTM D1922
Elmendorf Tear Strength, TD 0.732 g/micron18.6 g/milASTM D1922
Film Tensile Strength at Break, MD >= 55.2 MPa>= 8000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
CTE, linear  67.0 µm/m-°C
@Temperature 50.0 - 70.0 °C
37.2 µin/in-°F
@Temperature 122 - 158 °F
MD; ASTM D696
 80.0 µm/m-°C
@Temperature 50.0 - 70.0 °C
44.4 µin/in-°F
@Temperature 122 - 158 °F
TD; ASTM D696
Specific Heat Capacity 1.09 J/g-°C0.261 BTU/lb-°FDuPont 990 test
Maximum Service Temperature, Air 107 °C225 °FContinuous
 175 °C347 °FShort Cycle
Minimum Service Temperature, Air -72.0 °C-97.6 °FContinuous
Shrinkage <= 5.0 %
@Temperature 170 °C
<= 5.0 %
@Temperature 338 °F
TD; ASTM D1204
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.46
@Temperature 30.0 °C
1.46
@Temperature 86.0 °F
nD; Abbe Refractometer; ASTM D-542
 
Descriptive Properties
Aging in Air> 3000 hours to embrittlement300°F Oven

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Tedlar® TTR10BG3 Transparent Polyvinyl Fluoride Film
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film
DuPont™ Tedlar® TWH20BS3 Satin White Polyvinyl Fluoride Film
DuPont™ Tedlar® SP TTR10AH9 Transparent Polyvinyl Fluoride Film
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film

PDU9309 / 138482

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.