DuPont™ Tedlar® TWH20BS3 Satin White Polyvinyl Fluoride Film
Categories:
Polymer
;
Film
;
Thermoplastic
;
Fluoropolymer
Material Notes:
Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety of chemicals, solvents, and staining agents.
Key Words:
PVF
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.71
g/cc
1.71
g/cc
ASTM D1505
Moisture Absorption at Equilibrium
<= 0.50 %
<= 0.50 %
ASTM D570
Moisture Vapor Transmission
0.860
cc-mm/m²-24hr-atm
2.18
cc-mil/100 in²-24hr-atm
ASTM E96
Thickness
50.8
microns
2.00
mil
Mechanical Properties
Metric
English
Comments
Film Elongation at Break, MD
>= 110 %
>= 110 %
ASTM D882
Secant Modulus, MD
2.65
GPa
385
ksi
ASTM D822
Impact
71.6
71.6
kJ/m; Spencer; ASTM D3420
Coefficient of Friction
0.18
0.18
Film:Metal; ASTM D1894
Tear Strength
146
kN/m
833
pli
Graves (initial), TD; ASTM D1004
195
kN/m
1110
pli
Graves (initial), MD; ASTM D1004
Elmendorf Tear Strength, MD
1.82
g/micron
46.2
g/mil
ASTM D1922
Elmendorf Tear Strength, TD
1.05
g/micron
26.6
g/mil
ASTM D1922
Film Tensile Strength at Break, MD
>=
62.1
MPa
>=
9000
psi
ASTM D882
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.50e+11
ohm-cm
@Temperature 100 °C
1.50e+11
ohm-cm
@Temperature 212 °F
ASTM D257
7.00e+14
ohm-cm
@Temperature 22.0 °C
7.00e+14
ohm-cm
@Temperature 71.6 °F
ASTM D257
Dielectric Constant
11
@Frequency 1000 Hz
11
@Frequency 1000 Hz
ASTM D150
Dielectric Strength
138
kV/mm
@Frequency 60 Hz
3500
kV/in
@Frequency 60 Hz
ASTM D150
Dissipation Factor
0.014
@Frequency 1000 Hz,
Temperature 22.0 °C
0.014
@Frequency 1000 Hz,
Temperature 71.6 °F
ASTM D150
0.016
@Frequency 10000 Hz,
Temperature 70.0 °C
0.016
@Frequency 10000 Hz,
Temperature 158 °F
ASTM D150
0.017
@Frequency 1000 Hz,
Temperature 70.0 °C
0.017
@Frequency 1000 Hz,
Temperature 158 °F
ASTM D150
0.034
@Frequency 10000 Hz,
Temperature 22.0 °C
0.034
@Frequency 10000 Hz,
Temperature 71.6 °F
ASTM D150
Thermal Properties
Metric
English
Comments
CTE, linear
83.0
µm/m-°C
@Temperature 50.0 - 70.0 °C
46.1
µin/in-°F
@Temperature 122 - 158 °F
TD; ASTM D696
97.0
µm/m-°C
@Temperature 50.0 - 70.0 °C
53.9
µin/in-°F
@Temperature 122 - 158 °F
MD; ASTM D696
Specific Heat Capacity
1.05
J/g-°C
0.251
BTU/lb-°F
DuPont 990 test
Maximum Service Temperature, Air
107
°C
225
°F
Continuous
175
°C
347
°F
Short Cycle
Minimum Service Temperature, Air
-72.0
°C
-97.6
°F
Continuous
Shrinkage
<= 5.0 %
@Temperature 170 °C
<= 5.0 %
@Temperature 338 °F
TD; ASTM D1204
Optical Properties
Metric
English
Comments
Refractive Index
1.46
@Temperature 30.0 °C
1.46
@Temperature 86.0 °F
n
D
; Abbe Refractometer; ASTM D-542
Descriptive Properties
Aging in Air
> 3000 hours to embrittlement
300°F Oven
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film
DuPont™ Tedlar® TWH15BL3 Low Gloss White Polyvinyl Fluoride Film
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film
PDU9310 / 138483
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.