Kaolite 2500-LI Gun is a 2500°F (1371°C) lightweight insulating castable that contains an intermediate-purity, calcium aluminate cement. Total iron content of <_ 1.0% enables its use where hydrogen or reducing atmospheres are present. Information provided by Thermal Ceramics Data has not been recently verified. Please contact manufacturer for current information. |