MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Kaolite 2500-LI Gunning Insulation Castables
Categories: Ceramic; Oxide

Material Notes: Kaolite 2500-LI Gun is a 2500°F (1371°C) lightweight insulating castable that contains an intermediate-purity, calcium aluminate cement. Total iron content of <_ 1.0% enables its use where hydrogen or reducing atmospheres are present.

Information provided by Thermal Ceramics

Data has not been recently verified. Please contact manufacturer for current information.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.025 - 1.17 g/cc0.03703 - 0.0423 lb/in³Fired at 1500°F
 1.025 - 1.17 g/cc0.03703 - 0.0423 lb/in³Fired at 2500°F
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00103 - 0.00172 GPa0.150 - 0.250 ksiDried 18-24 hours at 220°F; ASTM C133
 0.000827 - 0.00138 GPa
@Treatment Temp. 816 °C,
Time 18000 sec
0.120 - 0.200 ksi
@Treatment Temp. 1500 °F,
Time 5.00 hour
ASTM C133
 0.00172 - 0.00276 GPa
@Treatment Temp. 1370 °C,
Time 18000 sec
0.250 - 0.400 ksi
@Treatment Temp. 2500 °F,
Time 5.00 hour
ASTM C133
Compressive Strength 3.10 - 4.48 MPa450 - 650 psiDried for 18-24 hours at 220°F
 3.45 - 5.51 MPa500 - 799 psiFired 5 hours at 1500°F
 4.13 - 6.20 MPa599 - 899 psiFired 5 hours at 2500°F
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.268026 W/m-K
@Temperature 260 °C
1.86010 BTU-in/hr-ft²-°F
@Temperature 500 °F
 0.295405 W/m-K
@Temperature 538 °C
2.05011 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 0.324225 W/m-K
@Temperature 816 °C
2.25012 BTU-in/hr-ft²-°F
@Temperature 1500 °F
 0.354486 W/m-K
@Temperature 1093 °C
2.46013 BTU-in/hr-ft²-°F
@Temperature 1999 °F
Maximum Service Temperature, Air 1370 °C2500 °F
Shrinkage  -1.00 - 0.50 %
@Temperature 1370 °C,
Time 18000 sec
-1.00 - 0.50 %
@Temperature 2500 °F,
Time 5.00 hour
ASTM C113
 0.20 - 0.50 %
@Temperature 816 °C,
Time 18000 sec
0.20 - 0.50 %
@Temperature 1500 °F,
Time 5.00 hour
ASTM C113
 0.00 - 0.20 %
@Treatment Temp. 104 °C
0.00 - 0.20 %
@Treatment Temp. 220 °F
Dried 18-24 hours; ASTM C113
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Al2O3 44 %44 %
Alkalis 1.3 %1.3 %
CaO 17 %17 %
Fe2O3 0.90 %0.90 %
MgO 0.20 %0.20 %
SiO2 35 %35 %
TiO2 1.8 %1.8 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Thermal Ceramics Kaolite 2300-LI Gunning Insulation Castables
Thermal Ceramics Kaolite 1800 Super Lightweight Insulating Castables
Thermal Ceramics Kaocast 3000 Dense Castable

CTHERM046 / 2366

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.