VESTAKEEP 4000 CF30 is a carbon fiber reinforced (30%) polyether ether ketone for injection molding. The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP 4000 CF30 are self-extinguishing. VESTAKEEP 4000 CF30 can be processed by common injection molding machines for thermoplastics.Information provided by Evonik |