MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Abatron AboCast/AboCure 4-4/50-3 Casting Epoxy for Tooling
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.

Main Advantages:

  • Easy ratios
  • Long pot life
  • Large castings
  • Low exotherm

Main Drawbacks:

  • Very slow for very thin castings (<0.5 inch)
  • Lower chemical resistance

Processing: 100/20 ratio. Room temperature cure 8 to 48 hours, optional post-cure 2 to 4 hours at 80 to 110°C.

Information provided by Abatron.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.10 - 0.50 %24-200 hours
Linear Mold Shrinkage 0.0010 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 85
Tensile Strength at Break 5200 psi
Elongation at Break 3.6 %
Flexural Strength 7200 psi
Compressive Strength 12500 psi
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.00140 - 0.00160 cal cm/sec-cm²-°C
Maximum Service Temperature, Air 65.0 - 70.0 °C
 93.0 °CDeflection temperature after post-cure
 
Processing PropertiesOriginal ValueComments
Pot Life 120 - 180 min
@Temperature 25.0 °C
1-2 lbs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay LTM® 10 Epoxy Resin
Solvay LTF 318B
Solvay CYFORM® 22 Epoxy Tooling Prepreg
Quantum Composites LYTEX® 4182 50-55% Carbon Fiber Reinforced Epoxy SMC
Lord Adhesives Circalok™ EP-729 Epoxy Board Level Encapsulant

PABKW000 / 22041

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.