MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DESMOPHEN® 670 BA Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Slightly branched hydroxyl-bearing polyester. As a co-reactant primarily with Desmodur® N 75 and N 3390 in the formulation of weather-stable flexible coatings.

Properties / Applications: Combined with Desmodur® N 75 or N 3390, Desmophen® 670 BA yields films with very good weather stability and excellent low temperature flexibility. Such coatings are mainly used to coat plastics and are force-dried, e.g. at 80 °C. Desmophen® 670 BA can also be added to other two-component polyurethane systems to improve their flexibility.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccDIN EN ISO 2811-2
Volatiles 19 - 21 %1 g resin/1 h 125 °C, convection oven; DIN EN ISO 3251
Viscosity 2600 - 3400 cPDIN EN ISO 3219/A.3
 
Chemical PropertiesOriginal ValueComments
Acid Value 0.80 - 2.8[mg KOH/g]; DIN EN ISO 2114
 
Thermal PropertiesOriginal ValueComments
Flash Point 32.0 °CDIN EN ISO 2719
 
Processing PropertiesOriginal ValueComments
Moisture Content >= 0.10 %DIN 51 777/1
 
Descriptive Properties
Color<150Hazen, DIN EN 1557
Content3.2-3.8%Hydroxyl, DIN 53 240/2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DESMOPHEN® 651 MPA Polyurethane
Covestro Desmodur® HL BA Polyurethane
Covestro DESMOPHEN® 650A-65 PMA Polyurethane
Covestro DESMOPHEN® 650 MPA Polyurethane
Covestro DESMOPHEN® 631 MPA Polyurethane

PCOVEST0737 / 202520

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.