Characterization: Desmophen 631 MPA is a saturated polyester resin. Properties / Applications: Desmophen 631 MPA polyester is a co-reactant for Desmodur® N 3200 polyisocyanate in two-component polyurethane coatings where higher solids (lower VOC) are needed. These coatings posses outstanding gloss retention, light stability and good chemical and abrasion resistance. As with any product, use of Desmophen 631 MPA in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. Information provided by Covestro |