MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DESMOPHEN® 631 MPA Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Desmophen 631 MPA is a saturated polyester resin.

Properties / Applications: Desmophen 631 MPA polyester is a co-reactant for Desmodur® N 3200 polyisocyanate in two-component polyurethane coatings where higher solids (lower VOC) are needed. These coatings posses outstanding gloss retention, light stability and good chemical and abrasion resistance. As with any product, use of Desmophen 631 MPA in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Solids Content 73 - 77 %
Viscosity 10000 - 25000 cP
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 3.1[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Flash Point 50.0 °CSetaflash
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 3.0
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %
 
Descriptive Properties
AppearanceYellowish liquid
Content6.4%OH
Hydroxyl number200-220

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DESMOPHEN® 650 MPA Polyurethane
Covestro DESMOPHEN® 650A-65 PMA Polyurethane
Covestro DESMOPHEN® 651 MPA Polyurethane
Covestro DESMOPHEN® 1200 BA Polyurethane
Covestro DESMOPHEN® 1300 BA Polyurethane

PCOVEST0733 / 202516

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.