MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BCC Products BC 8086 Urethane Casting
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: BC 8086 is a rapid setting, low viscosity, polyurethane casting system. It exhibits a working life of 45 seconds and obtains a demoldable hardness at 7 - 10 minutes. Some of the features include: non-sensitive to moisture after cure, paintable (non oil base), will readily bond to itself, moderate heat resistance, excellent machinablilty and surface scribing, no settling components, and no premixing required.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792-66
Brookfield Viscosity 200 - 400 cP
@Temperature 23.9 °C
Mixed; ASTM D2393
Linear Mold Shrinkage 0.010 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 79ASTM D2240
Tensile Strength, Ultimate 5980 psiASTM D638
Elongation at Break 6.4 %ASTM D638-72
Flexural Strength 8810 psiASTM D790
Compressive Strength 6460 psiASTM D695
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 137 °F24 Hours at 75°F
 145 °F7 Days at 75°F
 
Processing PropertiesOriginal ValueComments
Cure Time 7.00 - 10.0 min
@Temperature 25.0 °C
demold time
Gel Time 0.750 min
@Temperature 24.0 °C
4 oz. mass; ASTM D2471-71
 
Descriptive Properties
Mix Ratio100:88 by weight, 100:100 by volume, resin/harder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BCC Products BC 8400 Urethane Casting
BCC Products BC 8165 Urethane Casting
BCC Products SLO-KAST BC 8009 Urethane Casting
BCC Products DP-11-90 Urethane Casting
BCC Products BC 8405 Urethane Casting

PBCC050 / 107277

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.