MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta NP572 Epoxy Glass Laminate Sheet, NEMA G-11
Categories: Polymer; Thermoset; Epoxy

Material Notes: NP572 is a high strength, medium weave glass epoxy laminate that retains a minimum of 50 percent of its room temperature flexural strength when tested at 150ºC and its Tg is guaranteed to be 180°C or greater. Typical applications include electrical equipment subjected to elevated temperatures. NP572 is certifiable to IEC 60216-3, IEEE STD 98-2002 and ASTM D2304 for Class H insulation in electrical devices. NP572 is also certifiable to MIL-I-24768/3, Type GEB and IEC 60893-3-2-EP GC 308.

Information provided by Norplex-Micarta

Key Words: Glass Fiber, Epoxy, Micarta, NEMA G-11, ASTM D709 Type IV Grade G-11, MIL-I-24768/3 GEB, IEC 60216 Class H, IEEE 98-2002 Class H, IEC 60893-3-2-EP GC 308
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.89 g/cc
@Thickness 12.7 mm
ASTM D792
Moisture Absorption 0.200 %
@Thickness 1.57 mm
ASTM D570 Condition A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 108
@Thickness 6.35 mm
ASTM D785
Tensile Strength 35000 psi
@Thickness 3.17 mm
CrossWise; ASTM D638 Condition A
 47300 psi
@Thickness 3.17 mm
LengthWise; ASTM D638 Condition A
Flexural Strength 53000 psi
@Thickness 1.57 mm
CrossWise; ASTM D790 Condition A
 68500 psi
@Thickness 1.57 mm
LengthWise; ASTM D790 Condition A
Compressive Strength 72100 psi
@Thickness 12.7 mm
Flatwise; ASTM D695 Condition A
Shear Strength 25200 psi
@Thickness 1.57 mm
perpendicular; ASTM D732 Condition A
Izod Impact, Unnotched 10.3 ft-lb/in
@Thickness 12.7 mm
CrossWise; ASTM D256 Condition E-48/50
 12.5 ft-lb/in
@Thickness 12.7 mm
LengthWise; ASTM D256 Condition E-48/50
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.1
@Thickness 1.57 mm,
Frequency 1e+6 Hz
ASTM D150 Condition D-24/23
Dielectric Strength 680 V/mil
@Thickness 1.57 mm
ASTM D149 Condition A
 760 V/mil
@Thickness 1.57 mm
ASTM D149 Condition D-48/50
Dielectric Breakdown 69000 V
@Thickness 1.57 mm
ASTM D149 Condition A
Dissipation Factor 0.018
@Thickness 1.57 mm,
Frequency 1e+6 Hz
ASTM D150 Condition D-24/23
Arc Resistance 185 sec
@Thickness 3.17 mm
ASTM D495 Conition A
 
Thermal PropertiesOriginal ValueComments
Transformation Temperature, Tg 180 °C
@Thickness 12.7 mm
DMA
Flammability, UL94 V-0
@Thickness 1.57 mm
 
Descriptive Properties
Bonding Strength1800[lb]; 0.5"; ASTM D229 Condition D-48/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Norplex-Micarta MC511A Epoxy Glass Laminate Sheet, NEMA G-11
Norplex-Micarta MC511AF Epoxy Glass Laminate Sheet, NEMA G-11
Norplex-Micarta MC511FR Epoxy Glass Laminate Sheet, NEMA FR-5
Norplex-Micarta NP511 Epoxy Glass Laminate Sheet, NEMA G-11
Norplex-Micarta NP511EM Epoxy Glass Laminate Sheet, NEMA G-11

PNORPM057 / 192814

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.