MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Misumi Z3234 Chromium Copper
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent mechanical strength and abrasion resistance at high temperatures. Used in welding electrodes, seam welding wheels, switch gears, electrode holder jaws, cable connectors, current carrying arms and shafts, circuit breaker parts, molds, spot welding tips, flash welding electrodes, electrical and thermal conductors requiring strength, switches and contacts.

Information provided by MISUMI Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.89 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 125
Tensile Strength, Ultimate >= 380 MPa
Elongation at Break >= 15 %
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.0000020 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.800 cal cm/sec-cm²-°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 7091 ADHESIVE SEALANT
ASTM A230 Carbon Steel Wire
Parker Chomerics THERM-A-GAP™ GEL 30 High Performance Fully Cured Dispensable Gel
ChevronTexaco Vistac® ISO 32 Rock Drill Oil
ChevronTexaco RPM® SAE 15W-40 Gas Engine Oil

NMISUM954 / 178119

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.