MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Vistac® ISO 32 Rock Drill Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Rock Drill Oils Vistac are designed to give maximum protection to percussion rock drills.

They are formulated from highly refined, high viscosity index, paraffinic base stocks and additives, which provide all of the performance characteristics, expected of a superior rock drill oil. As indicated by part of the name, Vistac, the additives provide an unusual adhesive or tacky quality.

Chevron Rock Drill Oils Vistac are formulated to meet the critical lubrication demands of percussion rock drills. Their superior extreme pressure performance provides protection for the rock drill piston, rifle bar and nut against the heavy shock loads typical of rock drill service. The adhesiveness and emulsification tendency of these oils provide a tenacious lubricant film on the rock drills moving parts which will not be washed off by incidental water that is common in the compressed air which drives the piston in this application.

The oils also provide excellent rust and corrosion protection, which is important in light of the corrosive environments in which many rock drills are used. Chevron Rock Drill Oils Vistac contain no chlorinated additives and are completely ashless, minimizing environmental and disposal considerations.

Additionally, since rock drills are frequently used in mining environments where ventilation is limited, the low odor and toxicity of these lubricants are added benefits.

Applications

Chevron Rock Drill Oils Vistac have proven excellence in all air-operated tools, such as jackhammers, drifters, etc.

The wide viscosity range of this product line makes them suitable for use under many different climatic conditions.

The additive package of these oils provides many performance characteristics, which lend themselves well to the lubrication of enclosed gears, and all types of industrial plain and anti-friction bearings.

Their tacky quality makes these oils suitable for oncethrough applications; e.g. lubrication of chain drives.

They meet the performance requirements of many rock drill manufacturers, such as Ingersoll-Rand, Gardner-Denver, Sullivan, etc.

Chevron Rock Drill Oils Vistac ISO 46, 100, 150, 220, and 320 meet all of the specifications of Ingersoll-Rand and Sullivan for light, medium, and heavy rock drill oils.

Key Words: CPS Number: 232342; MSDS Number: 6752
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 23.2 °23.2 °
Viscosity Measurement 4040Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 158 SUS158 SUS
Saybolt Viscosity at 210°F 42 SUS42 SUS
Kinematic Viscosity at 40°C (104°F) 30.4 cSt30.4 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 4.6 cSt4.6 cStASTM D445
 
Mechanical PropertiesMetricEnglishComments
Falex Load Test 1.59e+6 g3500 lb
Timken Test 24900 g55.0 lb
 
Thermal PropertiesMetricEnglishComments
Pour Point -42.0 °C-43.6 °FASTM D97
Flash Point 190 °C374 °FASTM D92
 
Descriptive Properties
Steam emulsion number>1200

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 32341 Phenolic Resin
Sumitomo Bakelite Durez® 32340 Phenolic Resin
Rogers Arlon 23234R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Phosphate Rock
Misumi Z3234 Chromium Copper

WCHEV343 / 74958

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.