MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kraton® G1652 E (SEBS) Linear Block Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton G1652 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass. It is supplied from Europe in the physical form shown:
Kraton G1652 EU - supplied as undusted fluffy crumb
Kraton G1652 ES - supplied as fluffy crumb dusted with amorphous silica

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton G1652 E is used as a modifier of bitumen or thermoplastics and in compound formulations. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants and coatings.

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Impact Modification; Medical; Packaging and Polymod; and Personal Care

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccISO 2781
Volatiles <= 0.60 %KM 04
Brookfield Viscosity 400 - 530 cP
@Temperature 25.0 °C
25% Toluene solution
Melt Flow 6.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ISO 1133
Ash 0.70 - 1.1 %ISO 247
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 6910 seconds.; ASTM D 2240
Tensile Strength, Ultimate 31.03 MPaASTM D412
Elongation at Break 500 %ASTM D412
300% Modulus 0.00483 GPa
@Strain 300 %
ASTM D412
 
Descriptive Properties
ContentAntioxidant>0.03%, KM 08
 Polystyrene28.2-30%, KM 03, polystyrene content measured on finished product after hydrogenation
 Total Extractables<1.0%, KM 05

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® G1650 E (SEBS) Linear Block Copolymer
Kraton® FG1924 G (SEBS) Linear Block Copolymer
Kraton® G1654 E (SEBS) Linear Block Copolymer
Kraton® G1657 M (SEBS) Linear Block Copolymer
Kraton® G7723X

PKRA0250 / 49085

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.