MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Polystyrol® 2710 Impact Grade Polystyrene (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Special high-impact grade for refrigerators and the packaging sector. Particularly resistant to stress cracking.

Data was collected by ISO methods and provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Water Absorption 0.10 %0.10 %
Moisture Absorption at Equilibrium 0.10 %0.10 %
Linear Mold Shrinkage, Flow 0.0055 cm/cm0.0055 in/in
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
4.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 21.0 MPa3050 psi
Elongation at Break 35 %35 %
Elongation at Yield 1.7 %1.7 %
Tensile Modulus 1.50 GPa218 ksi
Charpy Impact Unnotched NBNB
 12.0 J/cm²
@Temperature -30.0 °C
57.1 ft-lb/in²
@Temperature -22.0 °F
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+13 ohm1.00e+13 ohm
Dielectric Constant  2.5
@Frequency 100 Hz
2.5
@Frequency 100 Hz
 2.5
@Frequency 1e+6 Hz
2.5
@Frequency 1e+6 Hz
Dissipation Factor 0.00010
@Frequency 1e+6 Hz
0.00010
@Frequency 1e+6 Hz
Comparative Tracking Index 500 V500 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Temperature 20.0 °C
55.6 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C189 °F
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C172 °F
Vicat Softening Point 89.0 °C192 °F
Flammability, UL94 HB
@Thickness 3.18 mm
HB
@Thickness 0.125 in
Oxygen Index 18 %18 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PSI 7240 High Impact Polystyrene
BASF Polystyrol® 456 F Impact Grade Polystyrene (Europe)
BASF Polystyrol® 455 F WU Impact Grade Polystyrene (Europe)
Menzolit Menzolit® SMC 0400 Unsaturated Polyester UP
Ineos Styrenics 158K High-Heat Polystyrene Crystal Resin (Global)

PSF184 / 66765

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.