MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ametek P430L P/M Stainless Steel, Sintered from 6.2 g/cc Green Density
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.

Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for 45 minutes. Sintered properties below were determined using transverse rupture bars. Compacting pressure 38 tsi. Green strength 1200 psi. Dimensional change from die size -0.8%.

Information provided by Ametek Specialty Metal Products.

Key Words: Powder metallurgy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 340 MPa49300 psi
Elongation at Break 1.5 %1.5 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.020 %0.020 %
Chromium, Cr 17 %17 %
Iron, Fe 82 %82 %as balance
Manganese, Mn 0.20 %0.20 %
Phosphorus, P 0.010 %0.010 %
Silicon, Si 0.90 %0.90 %
Sulfur, S 0.020 %0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™ (ASTM XM-8; UNS S43035)
Ametek P434L P/M Stainless Steel, Sintered from 6.2 g/cc Green Density
ATI Allegheny Ludlum AL 440C™ Martensitic Stainless Steel, UNS S44004
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 538°C Temper
ATI Allegheny Ludlum T-436 Ferritic Stainless Steel, UNS S43600

NMA045 / 18142

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.