MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT HANSA LPF 716 Organo-modified polysiloxane
Categories: Other Engineering Material

Material Notes: Description: This product confers waterproofing effects on leather materials like footwear, sportive garment and gloves with innovative water-repellent solutions environment friendly (fluorine free).

Key Features

  • Imparts water-proofing behaviour
  • Very good compatibility with organic compounds
  • Fluorocarbon-free
  • The viscosity may change by ageing but this does not impact the product quality.
Key Applications
  • Wet-end processes, especially in re-fatting
Application: HANSA® LPF 716 is a carboxy-functional polydimethylsiloxane which can be used for the water-proofing treatment of leather. It is particularly suitable in wet-end processes, especially during refatting. HANSA® LPF 716 is not soluble in water. It can be dissolved in alcohol; the optimal application amount must be adjusted to the desired effect. HANSA® LPF 716 can be used in combination with HANSA® WS 1175 in order to achieve an even better waterproofing effect.

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Brookfield Viscosity 5000 - 15000 cP5000 - 15000 cP
Storage Temperature <= 40.0 °C<= 104 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceSlightly yellowish liquid
ChemistrySide modified carboxy functional polydimethylsiloxane
IonicityAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL228 / 314711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.