System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
XXX Phenolic Laminate
Categories:
Polymer
;
Thermoset
;
Filled/Reinforced Thermoset
;
Phenolic
Material Notes:
Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.
Information provided by Aurora Technologies.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.0470
lb/in³
Water Absorption
0.50 %
Mechanical Properties
Original Value
Comments
Hardness, Rockwell M
110
Tensile Strength, Ultimate
20000
psi
Flexural Strength
23000
psi
Compressive Strength
38000
psi
Shear Strength
12000
psi
Izod Impact, Notched
0.800
ft-lb/in
Electrical Properties
Original Value
Comments
Volume Resistivity
3.00e+13
ohm-cm
Surface Resistance
7.00e+11
ohm
Dielectric Constant
4.9
@Frequency 1e+6 Hz
Dielectric Strength
475
V/mil
Dielectric Breakdown
65000
V
Dissipation Factor
0.042
@Frequency 1e+6 Hz
Arc Resistance
124
sec
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
140
°C
Mechanical
140
°C
Electrical
Descriptive Properties
Color
Natural
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
G-3 Fiberglass Phenolic Laminate Sheet
CE Phenolic Laminate
Ensinger Tecapeek® Polyetheretherketone (PEEK)
Aluminum 6063-T5
Elektro-Isola Etronit IIQ R XX Phenolic, Paper Reinforcement, Yellow, Sheets
PGLAM24 / 41895
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.