Key Features:- One part, no mix system
- Cures at room or elevated temperatures
- Relatively fast curing
- Good electrical conductivity
Master Bond X5SC is a solvent based elastomeric system with superb electrical conductivity. It has a paste-like consistency and is very easy to use. When used as an adhesive, it is simply applied in a thin layer to one of the substrates. The surfaces are then mated and fixtured, and the product is allowed to cure. Additionally, it can be applied in a similar manner as a coating material for shielding. Curing in either case is generated by the evaporation of the solvent. RoHS Compliant.Information provided by Master Bond. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |