MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Master Bond X5SC One Component Silver Filled Elastomeric Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive, Flexible; Epoxy, Electrically Conductive

Material Notes: Key Features:
  • One part, no mix system
  • Cures at room or elevated temperatures
  • Relatively fast curing
  • Good electrical conductivity
Master Bond X5SC is a solvent based elastomeric system with superb electrical conductivity. It has a paste-like consistency and is very easy to use. When used as an adhesive, it is simply applied in a thin layer to one of the substrates. The surfaces are then mated and fixtured, and the product is allowed to cure. Additionally, it can be applied in a similar manner as a coating material for shielding. Curing in either case is generated by the evaporation of the solvent. RoHS Compliant.

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.91 g/cc
Water Absorption <= 0.50 %
@Time 86400 sec
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.0010 ohm-cm
@Temperature 23.9 °C
Surface Resistance <= 0.0010 ohm
@Temperature 75.0 °C
Shielding Effectiveness 90 - 110 dB
@Frequency 1000 - 1.00e+9 Hz
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.44 - 1.73 W/m-K
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -80.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 - 12.0 hour
@Temperature 23.9 °C
option 2
 60.0 - 90.0 min
@Temperature 65.6 °C
option 1
Shelf Life 3.00 Month
@Temperature 23.9 °C
in original, unopened containers
 
Descriptive Properties
ColorGray
Viscositypaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTM984 / 187002

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.