MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Total Finaplas® 1571 Copolymer Syndiotactic Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: FINAPLAS® 1571 is a syndiotactic form of copolymer polypropylene via ATOFINA proprietary technology. Syndiotactic is a lower melting, lower crystallinity form of polypropylene. FINAPLAS® 1571 complies with FDA regulations Title 21 CFR Section 177.1520 (c) 3.1 and may be used under these provisions for food contact and packaging.

Application

FINAPLAS® 1571 is a high melt strength grade recommended for extruded sheet and film constructions.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 g/cc0.0314 lb/in³ASTM D1505
Melt Flow 10 g/10 min10 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 15.9 MPa2300 psiASTM D638
Elongation at Break 310 %310 %ASTM D790
Elongation at Yield 10 %10 %ASTM D790
Tensile Modulus 0.490 GPa71.0 ksiASTM D638
Flexural Modulus 0.379 GPa55.0 ksiASTM D638
Izod Impact, Notched 6.41 J/cm12.0 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FDSC-2 Differential Scanning Calorimeter
 
Optical PropertiesMetricEnglishComments
Haze 4.6 %4.6 %ASTM D1003
Yellow Index -2.30 %-2.30 %ASTM D1925
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Finaplas® 1471 Copolymer Syndiotactic Polypropylene
Total Finaplas® 1251 Copolymer Syndiotactic Polypropylene
Arkema Orevac® SM7-001-sPP Maleic Anhydride modified Polypropylene
Borealis Borsoft™ SF203CF Soft Polypropylene Copolymer for Extrusion Coating
Total PPR 8650 Polypropylene, Random Copolymer

PFINAA150 / 38586

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.