MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.17 - 1.62 g/cc0.0423 - 0.0585 lb/in³Average value: 1.38 g/cc Grade Count:60
Filler Content 10.0 - 30.0 %10.0 - 30.0 %Average value: 18.1 % Grade Count:8
Water Absorption 0.0600 - 0.300 %0.0600 - 0.300 %Average value: 0.137 % Grade Count:6
Moisture Absorption at Equilibrium 0.0600 - 0.150 %0.0600 - 0.150 %Average value: 0.112 % Grade Count:5
Water Absorption at Saturation 0.200 - 0.400 %0.200 - 0.400 %Average value: 0.300 % Grade Count:3
Maximum Moisture Content 0.02000.0200Average value: 0.0200 Grade Count:6
 0.200 - 0.200
@Temperature 120 - 120 °C
0.200 - 0.200
@Temperature 248 - 248 °F
Average value: 0.200 Grade Count:1
 0.200 - 0.200
@Time 299 - 299 sec
0.200 - 0.200
@Time 0.0830 - 0.0830 hour
Average value: 0.200 Grade Count:1
Linear Mold Shrinkage 0.000500 - 0.0100 cm/cm0.000500 - 0.0100 in/inAverage value: 0.00514 cm/cm Grade Count:40
Linear Mold Shrinkage, Transverse 0.00500 - 0.00800 cm/cm0.00500 - 0.00800 in/inAverage value: 0.00640 cm/cm Grade Count:5
Melt Flow 3.20 - 42.0 g/10 min3.20 - 42.0 g/10 minAverage value: 20.3 g/10 min Grade Count:31
Ash 13.0 - 18.0 %
@Temperature 625 - 625 °C
13.0 - 18.0 %
@Temperature 1160 - 1160 °F
Average value: 15.5 % Grade Count:1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 95.0 - 11995.0 - 119Average value: 111 Grade Count:8
Tensile Strength, Ultimate 48.0 - 148 MPa6960 - 21500 psiAverage value: 90.2 MPa Grade Count:38
Tensile Strength, Yield 48.0 - 114 MPa6960 - 16500 psiAverage value: 83.5 MPa Grade Count:23
Elongation at Break 2.00 - 200 %2.00 - 200 %Average value: 9.63 % Grade Count:47
Elongation at Yield 3.00 - 8.00 %3.00 - 8.00 %Average value: 4.20 % Grade Count:3
Modulus of Elasticity 0.860 - 13.1 GPa125 - 1900 ksiAverage value: 6.23 GPa Grade Count:15
Flexural Yield Strength 85.0 - 228 MPa12300 - 33000 psiAverage value: 140 MPa Grade Count:45
Flexural Modulus 1.72 - 12.4 GPa250 - 1800 ksiAverage value: 5.16 GPa Grade Count:54
Flexural Strain at Yield 3.00 - 4.70 %3.00 - 4.70 %Average value: 3.73 % Grade Count:3
Izod Impact, Notched 0.427 - 10.8 J/cm0.800 - 20.2 ft-lb/inAverage value: 1.97 J/cm Grade Count:39
 0.588399 - 0.588399 J/cm
@Temperature -30.0 - -30.0 °C
1.10231 - 1.10231 ft-lb/in
@Temperature -22.0 - -22.0 °F
Average value: 0.950 J/cm Grade Count:1
 1.01 - 1.07 J/cm
@Temperature -20.0 - -20.0 °C
1.89 - 2.00 ft-lb/in
@Temperature -4.00 - -4.00 °F
Average value: 0.950 J/cm Grade Count:2
 1.01 - 1.07 J/cm
@Thickness 3.18 - 3.18 mm
1.89 - 2.00 ft-lb/in
@Thickness 0.125 - 0.125 in
Average value: 0.950 J/cm Grade Count:2
Izod Impact, Unnotched 7.00 - 5340 J/cm13.1 - 10000 ft-lb/inAverage value: 8.13 J/cm Grade Count:5
Izod Impact, Notched (ISO) 5.80 - 13.0 kJ/m²2.76 - 6.19 ft-lb/in²Average value: 9.21 kJ/m² Grade Count:15
 6.00 - 11.0 kJ/m²
@Temperature -30.0 - -30.0 °C
2.86 - 5.23 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 9.14 kJ/m² Grade Count:7
Izod Impact, Unnotched (ISO) 35.0 - 40.0 kJ/m²16.7 - 19.0 ft-lb/in²Average value: 36.3 kJ/m² Grade Count:4
 35.0 - 80.0 kJ/m²
@Temperature -30.0 - -30.0 °C
16.7 - 38.1 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 47.0 kJ/m² Grade Count:5
Charpy Impact Unnotched 3.00 - 7.00 J/cm²14.3 - 33.3 ft-lb/in²Average value: 4.75 J/cm² Grade Count:8
 4.00 - 5.00 J/cm²
@Temperature -30.0 - -30.0 °C
19.0 - 23.8 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 4.60 J/cm² Grade Count:5
Charpy Impact, Notched 0.600 - 1.50 J/cm²2.86 - 7.14 ft-lb/in²Average value: 1.04 J/cm² Grade Count:8
 0.900 - 1.00 J/cm²
@Temperature -30.0 - -30.0 °C
4.28 - 4.76 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.975 J/cm² Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+13 - 1.00e+17 ohm-cm1.00e+13 - 1.00e+17 ohm-cmAverage value: 1.79e+16 ohm-cm Grade Count:10
Surface Resistance 1.00e+15 - 1.00e+17 ohm1.00e+15 - 1.00e+17 ohmAverage value: 1.34e+16 ohm Grade Count:8
Dielectric Constant 3.10 - 4.003.10 - 4.00Average value: 3.49 Grade Count:8
Dielectric Strength 20.0 - 34.0 kV/mm508 - 864 kV/inAverage value: 28.0 kV/mm Grade Count:7
Dissipation Factor 0.00130 - 0.01450.00130 - 0.0145Average value: 0.00987 Grade Count:5
Comparative Tracking Index 150 - 600 V150 - 600 VAverage value: 275 V Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.4 - 450 µm/m-°C13.0 - 250 µin/in-°FAverage value: 134 µm/m-°C Grade Count:8
CTE, linear, Transverse to Flow 35.0 - 80.0 µm/m-°C19.4 - 44.4 µin/in-°FAverage value: 57.0 µm/m-°C Grade Count:5
Melting Point 220 - 225 °C428 - 437 °FAverage value: 224 °C Grade Count:10
Deflection Temperature at 0.46 MPa (66 psi) 105 - 213 °C221 - 415 °FAverage value: 161 °C Grade Count:28
Deflection Temperature at 1.8 MPa (264 psi) 62.8 - 195 °C145 - 383 °FAverage value: 133 °C Grade Count:51
Vicat Softening Point 123 - 190 °C253 - 374 °FAverage value: 145 °C Grade Count:9
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:27
Glow Wire Test 750 - 850 °C1380 - 1560 °FAverage value: 783 °C Grade Count:3
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 245 - 304 °C473 - 580 °FAverage value: 263 °C Grade Count:10
Melt Temperature 220 - 316 °C428 - 600 °FAverage value: 259 °C Grade Count:35
Mold Temperature 38.0 - 121 °C100 - 250 °FAverage value: 80.1 °C Grade Count:35
Drying Temperature 82.2 - 121 °C180 - 250 °FAverage value: 109 °C Grade Count:32
Moisture Content 0.000 - 0.0200 %0.000 - 0.0200 %Average value: 0.0191 % Grade Count:11
Dew Point -40.0 - -17.8 °C-40.0 - 0.000 °FAverage value: -30.4 °C Grade Count:4
Injection Pressure 34.5 - 172 MPa5000 - 25000 psiAverage value: 97.2 MPa Grade Count:5
Vent Depth 0.00127 - 0.0203 cm0.000500 - 0.00800 inAverage value: 0.00924 cm Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced

O3176a / 89080

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.