MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Go Yen Chemical DPHP
Categories: Other Engineering Material

Material Notes: Di(2-Propyl Heptyl) phthalate (DPHP) is a phthalate ester plasticiser based on isomeric C10 alcohols. DPHP is a nearly colourless, clear and practically anhydrous liquid with a hardly noticeable odour. It is soluble in the usual organic solvents and is miscible and compatible with all of the monomeric plasticisers commonly used in PVC. DPHP is almost insoluble in water. Owing to its low volatility, DPHP is quite suitable for higher temperature applications such as wire & cable and automotive interior trim. With excellent weather resistance, it makes DPHP a good choice for outdoor applications such as roofing membranes and tarpaulins. DPHP can be used to substitute DINP, of which the weather resistance is better and the cost is lower.

Advantages:

  • Excellent weather resistance
  • Good anti-fogging properties
  • Wonderful thermal aging properties
  • Smell lighter
  • Higher output of thermoplastic processing
  • With good compatibility with PVC
Usage:
  • Wires & Cables
  • Automotive
  • Leather
  • Roofing membranes
  • Tarpaulines
  • Outdoor PVC products

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.957 - 0.965 g/cc0.0346 - 0.0349 lb/inĀ³ASTM D4052
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.070<= 0.070[mg-KOH/g]; ASTM D1045
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %ASTM E203
 
Descriptive Properties
Color<40Pt-Co units (APHA) ASTM D5386
Composition?99.5%Ester content; ASTM D3465

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN896 / 267204

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.