MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kennametal Stellite Delcrome 316L Iron Alloy
Categories: Metal; Ferrous Metal; Superalloy

Material Notes: Corrosion resistant alloys with moderate to high metal to metal wear resistance.

Information provided by Kennametal Stellite™

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C >= 20>= 20
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 13 %<= 13 %
Chromium, Cr 18 %18 %
Iron, Fe >= 63.87 %>= 63.87 %as balance
Manganese, Mn 0.70 %0.70 %
Molybdenum, Mo 2.6 %2.6 %
Silicon, Si 1.8 %1.8 %
Tungsten, W <= 0.030 %<= 0.030 %
 
Descriptive Properties
Application TechniquePTA & laser deposition

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
FloMet 316L Stainless Steel
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel
Ametek 316L Stainless Steel Thermal Spray Powder
Aluminum 7075-T73; 7075-T735x

NSTA4959 / 159891

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.