MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Cabot MONARCH® 430 Specialty Carbon Black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product highlights: MONARCH 430 specialty carbon black is an all-purpose regular color carbon black with low structure, allowing for lower viscosity or higher pigment loadings in a variety of applications.

Key applications: MONARCH 430 specialty carbon black is suitable for use in printing inks and other applications.
Printing inks: MONARCH 430 specialty carbon black is a general purpose pigment black that is broadly applicable in a variety of inks, including liquid, paste and lithographic inks. It provides good rub resistance of the image and viscosity and flow properties to the ink.
Other applications: This product is commonly used in adhesives and sealants, construction applications and in dispersions for both leather and textile colorants. The dispersibility of MONARCH 430 specialty carbon black depends on the equipment used and the formulation. A product with similar morphology, BLACK PEARLS® 430 specialty carbon black, is available in an easier to handle pelleted form.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.320 g/cc0.0116 lb/in³Tap; ASTM D-1513
Particle Mesh Size 325 Mesh325 Mesh<200 ppm residue; ASTM D-1514
 
Processing PropertiesMetricEnglishComments
Moisture Content 1.0 %1.0 %ASTM D-1509
 
Descriptive Properties
Iodine absorption82 mg/gCTM 23.4, Devolatilized
OAN75 cc/100gASTM D-2414
Product Formfluffy
Tint1.12ASTM D-3265

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT162 / 315897

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.