MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wanhua Chemical Wanthane® WHT-1198 Polyester Based TPU
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle time

Information provided by Wanhua Chemical Group Co., Ltd.

Key Words: FDA 21 CFR 177.1680, 177.2600; RoHS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9898ASTM D2240
Hardness, Shore D 6060ASTM D2240
Tensile Strength 40.0 MPa5800 psiASTM D412
Elongation at Break 430 %430 %ASTM D412
100% Modulus 17.0 MPa
@Strain 100 %
2470 psi
@Strain 100 %
ASTM D412
300% Modulus 32.0 MPa
@Strain 300 %
4640 psi
@Strain 300 %
ASTM D412
Tear Strength 170 kN/m970 pliASTM D624
 
Processing PropertiesMetricEnglishComments
Processing Temperature 195 - 215 °C383 - 419 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® D 60 E 4024 Polyester-Based TPU-High Performance Grade
Taiwan Sheen Soon Sheenthane® D6010 Thermoplastic Polyurethane Elastomer
Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether
Huntsman IROGRAN® A 85 P 4934 Ether-Based TPU-For Cable Industry
RTP Company RTP 1200 S-55D Ester-based Thermoplastic Polyurethane Elastomer

PWANTH905 / 156328

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.