MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ExxonMobil LD 617.LN Molding, Extrusion and Compounding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Product Description: LD 617.LN is a high flow, low density polyethylene homopolymer resin designed to provide excellent processability, flexibility and surface appearance. This multipurpose resin is performance engineered for applications such as housewares, overcaps and closures and concentrates.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Caps
  • Closures
  • Compounding
  • Food Packaging Containers
  • Houseware Articles
  • Injection Molding
  • Labware
  • Masterbatch Base Resin
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccExxonMobil Method
Melt Flow 26 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8615s; ASTM D2240
Hardness, Shore D 4215s; ASTM D2240
Tensile Strength at Break 1100 psiASTM D638
Tensile Strength, Yield 1600 psiASTM D638
Elongation at Break 120 %ASTM D638
Elongation at Yield 30 %ASTM D638
Flexural Modulus, 1% Secant 34000 psiASTM D790
Instrumented Impact Total Energy 12.0 ft-lb
@Temperature 22.8 °C
ASTM D3763
 14.0 ft-lb
@Temperature -20.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Melting Point 230 °FPeak Melting Temperature; ExxonMobil Method
Vicat Softening Point 183 °FASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil LD 637.LI Molding, Extrusion and Compounding Resin
ExxonMobil LD 516.LN Molding, Extrusion and Compounding Resin
Celanese 193 LDPE polymer for adhesives, automotive and compounds
ExxonMobil PP4031E2 Polypropylene Impact Copolymer
ExxonMobil PP7011L1 Polypropylene Impact Copolymer

PEXB057 / 37362

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.